Manganese value is more

18 views
Skip to first unread message

Chiranjeevi A

unread,
Nov 4, 2019, 6:14:11 AM11/4/19
to material...@googlegroups.com
Dear all,

We have LTCS Pipe(18" 160 sch A333 GR. 6), completed the flattening test. In the chemical analysis report shows manganese composition value is 1.49 but the range is between  . 290 to 1.06

Shall we accept dis. Experts share your opinions

Raghuram Bathula

unread,
Nov 4, 2019, 6:18:23 AM11/4/19
to Materials-Welding
max 1.35 is acceptable
btw did u succeed in flattening test?