ASME B31.3-2014- 331.2.6 Localized Heat Treatment after weld defect repair
35 views
Skip to first unread message
Anban
unread,
Oct 2, 2015, 11:57:18 PM10/2/15
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Dear Sirs
Pls advise if it is acceptable to ASME B31.3 Code.
Base Material Group - P1 x 10" dia x Sch 160. Weld Process- GTAW and FCAW.
Carried out RT after PWHT. Found 30mm defect at 9 o'clock position . Repaired.
Can i perform localized reheat treatment overlapping defect repaired location at least 100mm on both ends?
Thanks
Raghuram Bathula
unread,
Oct 3, 2015, 1:18:08 AM10/3/15
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials-Welding
As such there is no restriction in lieu of 360 ° banding, probably you may follow para 8.2.2.2 of API 570, but why do you go for this for a 10" dia pipe?