Experts,

Does the Code allows the Volumetric NDE for Welder Qualification for Unassigned material or similar composition?

I am aware about the exemption which Code states for some P number material and the Code case, but not sure about the Unassigned material/similar composition.

Looking forward for your as usual support.

Regards
Vino, Doha

Raghuram Bathula

unread,
Oct 1, 2015, 12:12:35 AM10/1/15
to Materials-Welding
Yes, the qualification is restricted to that unassigned material