Dear Ilkin,
The alloy 625 (Ni-Cr-Mo-Nb) for high temperature service 0-800 C and highly corrosive environment, rarely requires impact testing. ASTM B564 (UNS NO6625) does not state it as proof of its mechanical properties. If this is your case, at what temperature would you perform the Charpy test?
Better: in what temperature range is the service of this alloy located, in your case?