Please qualify separately in 2G and 5G to have the welder qualified for all positions.

 

Thanks.

 

 

Pradip Goswami.P.Eng, IWE.

Independent Consulting Welding & Metallurgical Engineering  Specialist

Saudi Aramco Approved Designated Project  Welding Engineer(DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: Hany Nabil <eng.han...@gmail.com>
Sent: May 30, 2021 3:15 AM
To: material...@googlegroups.com
Subject: welder qualification

 

Dear All,

It is known that the 6G position qualifies welder for all positions.

 If not possible to apply for a 6G position during WQT what are the two positions necessary to qualify a welder for all positions ?

 

 

 Best Regards,

 

 Eng. Hany Nabi

Welding Engineer

 Egypt Mobile: 002-01225622022

 

This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorized to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.


Virus-free. www.avg.com

Hany Nabil

unread,
May 30, 2021, 10:59:25 PM5/30/21
to material...@googlegroups.com

Dear All,

It is known that the 6G position qualifies welder for all positions.

 If not possible to apply for a 6G position during WQT what are the two positions necessary to qualify a welder for all positions ?


 Best Regards,

 Eng. Hany Nabi
Welding Engineer
 Egypt Mobile: 002-01225622022

This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

Paidi

unread,
May 31, 2021, 12:05:22 AM5/31/21
to material...@googlegroups.com
2G & 5G

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmRDNM44i9pQKAFGrp33_%3DfOZD7eror1ugpaunNLcFmvYw%40mail.gmail.com.


--
Thanks  & Best Regards,

Suresh Paidi


 

Vishwas Keskar

unread,
May 31, 2021, 12:29:18 AM5/31/21
to material...@googlegroups.com
Qualify in 2G and 5G 
Range Qualification  become All position

--

james gerald

unread,
Jun 1, 2021, 2:44:40 AM6/1/21
to material...@googlegroups.com
1. According to ASME Sec.IX and AWS D1.1, Alternatively 2G + 5G qualifies for ALL POSITIONS as 6G. Snap shot below.

Inline image

Inline image

2. According to API 1104 (Pipeline construction) no alternative provided.

Inline image


Thanks & Regards

J.Gerald Jayakumar