https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/732729f5-daa4-47f0-be88-367ad78c960bn%40googlegroups.com.
--
Thanks & Regards
K.Dinesh
Metallurgist
![]()
P.O. Box 1197, P.C 130, Muscat, Sultanate of Oman
Tel: +968 24501524, 24505590 (Ext.42), Mob: +968 99880633, Fax: +968 24503814
Email: dinesh@lonestaralpha.com , Web: www.lonestaralpha.com , Location: Click here for Location Map
Consider your environmental responsibility. Think before you print.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADder3PKdVJ45xOrwVAkekeMCPTNMjBvpF_EiRg1A8m%2BEV9PcA%40mail.gmail.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADder3PKdVJ45xOrwVAkekeMCPTNMjBvpF_EiRg1A8m%2BEV9PcA%40mail.gmail.com.
ASTM A297 Grade HP (Cr 24-28% & Ni 33-37%) is a heat-resistant stainless steel casting alloy commonly used in high-temperature
applications. ASTM A297 Grade HP (ASME sec II Part A and its UNS number is N08705) does not have a direct, one-to-one equivalent
in ASME standards and modified slightly for specific applications (example: pressure vessels, piping).
For practical purposes, in ASME codes, Grade HP would be referenced under SA-297 Grade HP for applications like furnace parts, heat
treatment equipment, or other high-temperature cast components. For a specific purpose like piping, it is referred to as ASME B16.5 -for
flanges.
C Sridhar.
-------------------------------------------------------------------------------------------------------------------------------------------------
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG5OBYGGbwwjMuWpKjF8nf21F%3DWQ2SUDh%3D6DBY9_-n9m2sE3Fw%40mail.gmail.com.