Hai,If your welder tested in 3G Position he can weld F,H & V Position.3G PQR Will support only Vertical Welding.If you need F&H position you need to establish New pqr with 2G position.Regards,Manikandan9791367960
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOScx2YEK2eVeOt%3D5PehBV3OtRdt%2B%2B_sB%2BaZu-JJGunaQ%40mail.gmail.com.
--
Thanks & Regards
J.Gerald Jayakumar
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P7Fs6c5nxzvj3o8SABXy9ePm0VZdkkxQV2n84iCYgU7Q%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P7Fs6c5nxzvj3o8SABXy9ePm0VZdkkxQV2n84iCYgU7Q%40mail.gmail.com.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BtZUbUEkFcN879PoNiKVoX-Gt7po2WbhhVuKamkAqFDh7mUOA%40mail.gmail.com.
Dear Dinesh,
Please Keep in Mind that Procedure Qualification & Welder Qualification have different Criterions for Range of Qualified Welding Position.
For Procedure Qualification, Clause 6.4(AWS D1.1 Ed:2020) explains about the Range of qualified Welding Position.(Directing to Table 6.1 for Plates & Table 10.8 for Tubular Products). You can refer Table 6.5 for PQR Essential variable changes Requiring Requalification.
For Performance Qualification, Clause 6.16.1(AWS D1.1 Ed:2020) explains about the Range of qualified Welding Position .(Directing to Table 6.10 for Plates & Table 10.12 for Tubular Products). You can refer Table 6.12 for Welding Personnel Performance Essential variable changes Requiring Requalification.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmODCwwk6ZLLcn%2BdxYATY49kaZa5RYtJn10iHwKq4du5bg%40mail.gmail.com.
Thanks & Regards
J.Gerald Jayakumar