S275JR to A36 WPS

87 views
Skip to first unread message

Vishnu Nandan

unread,
Mar 6, 2021, 6:08:06 AM3/6/21
to Materials & Welding
Hi
I have a qualified WPS for S275JR to S275JR. Can I use the same WPS to weld S275JR to A36.

Chris Sabu

unread,
Mar 6, 2021, 6:28:55 AM3/6/21
to material...@googlegroups.com
Even though procedure and everything will be same . S275JR is still unlisted in asme so you will need a seperate wps.

Regards

Chris

On Sat, Mar 6, 2021 at 15:08 Vishnu Nandan <nandan....@gmail.com> wrote:
Hi
I have a qualified WPS for S275JR to S275JR. Can I use the same WPS to weld S275JR to A36.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/51ecf34c-72ac-4780-a050-c0d45b9f41b6n%40googlegroups.com.
--
THANKS AND REGARDS
CHRIS SABU
0559695451

Vishwas Keskar

unread,
Mar 6, 2021, 7:23:52 AM3/6/21
to material...@googlegroups.com
Need separate PQR  as S275 is unassigned material 

On Sat, Mar 6, 2021 at 3:08 PM Vishnu Nandan <nandan....@gmail.com> wrote:
Hi
I have a qualified WPS for S275JR to S275JR. Can I use the same WPS to weld S275JR to A36.

--

Hani Al Masry

unread,
Mar 14, 2021, 11:42:45 PM3/14/21
to material...@googlegroups.com
No need A36 is equivalent to S275 Some times S235 Depend on its YS so no need to make new WPS 

Regards,
H.A 

Reply all
Reply to author
Forward
0 new messages