Corrosion Resistant Overlay over Carbon steel Preheat Requirements

32 views
Skip to first unread message

Vinoth kanna ramachandran

unread,
Jan 24, 2022, 4:36:54 AM1/24/22
to material...@googlegroups.com
Dear Welding Experts,

Preheat to be maintained or not for overlay of filler metal E309L-17 over carbon steel.
Any ASME clause referring to that, is highly appreciated.


Regards

Vinoth kanna
Gulf petrochemical Services I Oman

Vishwas Keskar

unread,
Jan 24, 2022, 6:04:45 AM1/24/22
to material...@googlegroups.com
what is Carbon steel thickness?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbO-YaO7gu01ayUO%2BceJoidxUNW_PTKyUM3VES-x_VSmc3U2w%40mail.gmail.com.

Vinoth kanna

unread,
Jan 24, 2022, 11:51:29 PM1/24/22
to material...@googlegroups.com
Dear,

Base material thickness 25mm (carbon steel) 
Ist layer using E309L
2nd layer using 316L 

Regards

Vinoth kanna