Dear All,

Please advise on what basis code Piping Inspection is done for process piping, Material Inspection is done through B31.3, but based on what we accept Ovality, Indendation like deformities.

Many Regards
Richard

raouf salhi

unread,
Feb 19, 2015, 3:41:50 AM2/19/15
to material...@googlegroups.com
Dear sir;

ovality ,deformities should be inspected according the factory fabrication code ( exp : for API 5L Gr B , according API 5L code ).

Regards
 
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbnFwoEcO1HmgXuP-21L%2Bo1Y2F7bmdJ8gKmQC%3Dofmi4t5hEqg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages