Dear expert, 
                      What is the meaning of dual grade lile 316/316L. Van anyone explain. 

duybien.com

unread,
Apr 29, 2024, 10:35:59 AMApr 29
to Materials & Welding
Dual grade complied type 316 and 316L.
- Chemical composing of %C: < 0.03%, and
- Min. YS: 205 MPa.

Regards

james gerald

unread,
Apr 29, 2024, 11:41:52 AMApr 29
to material...@googlegroups.com
316 -   C:0.08max  UTS : min 75ksi
316L - C:0.03 max UTS : min 70ksi

For dual certified both the conditions to be satisfied.

Dual certified 316/316L   - C: 0.03 max  UTS : min 75ksi

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/9a3429f5-740c-4d61-8d6e-cb63f4782390n%40googlegroups.com
.

Amol Betkar

unread,
Apr 29, 2024, 11:41:16 PMApr 29
to material...@googlegroups.com

Dear,

Dual grade stainless steel, like 316/316L, refers to a type of stainless steel that contains a mixture of two grades within one material. In this case, 316/316L indicates a combination of 316 stainless steel and its low carbon version, 316L.

316 stainless steel is a widely used grade known for its excellent corrosion resistance, particularly in acidic environments. It's commonly used in industries like marine, chemical processing, and pharmaceuticals.

316L is a variant of 316 stainless steel with a lower carbon content, which enhances its weldability. This makes it more suitable for applications where welding is involved, as it reduces the risk of carbide precipitation and consequent corrosion in the heat-affected zones of welded joints.

So, when you see "316/316L," it means you're getting the best of both worlds: the corrosion resistance of 316 stainless steel and the improved weldability of 316L. This dual-grade approach allows for greater versatility in various applications while maintaining the desired properties.

Regards,

Amol K.B



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9a3429f5-740c-4d61-8d6e-cb63f4782390n%40googlegroups.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

Jenish Mistry

unread,
Apr 30, 2024, 8:55:23 AMApr 30
to material...@googlegroups.com
Dear sir ,

Can you share references/Documents  @ james Gerald ? 



james gerald

unread,
Apr 30, 2024, 10:32:23 PMApr 30
to material...@googlegroups.com
Please ask some one in this group to send the MTC for dual certified grade of 316/316L as I do not have at this moment.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635

Reply all
Reply to author
Forward
0 new messages