TOFD of SS welding

38 views
Skip to first unread message

Manish Kumar

unread,
Feb 16, 2022, 10:22:20 PM2/16/22
to material...@googlegroups.com
Dear Sir,
Please advise as per ASME or other Demonstration of SS welding for TOFD possible or not.




Regards
Manish Kumar

George Dilintas

unread,
Feb 22, 2022, 10:59:20 PM2/22/22
to material...@googlegroups.com
with longitudinal waves only

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k5ET5rTKnzG%2B-6c5h42Jo1BBVwhT5dEYR6fCHNkSL3Yug%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Jenish Mistry

unread,
Feb 23, 2022, 12:08:00 AM2/23/22
to material...@googlegroups.com
Dear sir ,

Why not possible by transverse waves ??

please clarify..



--
Thanks for your best support.

Regards,
Jenish Mistry
09033476117

George Dilintas

unread,
Feb 23, 2022, 11:07:12 PM2/23/22
to material...@googlegroups.com
Because of attenuation due to coarse grain

Mohd Siraj

unread,
Mar 23, 2022, 7:21:51 AM3/23/22
to Materials & Welding
for austenite SS welding, pl use PAUT with DLA probe or DMA probe.

this brochure is for information only not recommended any brand or manufacturer
PAUT Solution for Austenitic Welds.pdf
Dual Matrix Array Probes for Welds.pdf