We have welded SA 240 TP310S to SA 240 TP310S plates with ER 310 filler wire. We get RT clear of the joints but get cracks in root & face bends. I am attaching photo of the same. Please give your expert advice for the same.
Thanks & regards,
Chirag Sandhane
Hi Chirag,
It seems the weld is sensitized. Please do micro examination to confirm the same.
Sent from Mail for Windows 10
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADP96MSoaRrwQ62A_5NwSxLHaDiwm2mW7qMH_1L8DRUr%3D11nDw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
I hope I may use your photograph in a presentation I am giving next month on cracking in welds and at a UK university.
Best wishes
Alan
Alan Denney
AKD Materials Consulting Ltd
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA724A2E032B4EE2BA957BFBB1E0E8B6%40homepg.
For more options, visit https://groups.google.com/d/optout.