Filler rod to weld titanium to SS304

71 views
Skip to first unread message

Pravin Poornachandran

unread,
Sep 5, 2022, 4:11:37 AM9/5/22
to 'Bijay' via Materials & Welding
Dear Expert,

Good day.

Can anyone share which filler to use to weld titanium to stainless steel 304? 

Understand that it’s difficult to weld this 2 material considering it’s thermal expansion is entirely different. 

Kindly advise.

Best regards 
Pravin 

Prakash Hegde

unread,
Sep 5, 2022, 4:21:25 AM9/5/22
to material...@googlegroups.com
No
You can not weld Ti to any Metal by.Arc. welding process
Regards
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7f6rX-P2STNFU%2BW0iZRbSq9uN8veyWzk4%3D9v4ghgTSTCg%40mail.gmail.com.

Pravin Poornachandran

unread,
Sep 5, 2022, 6:05:44 AM9/5/22
to material...@googlegroups.com
Dear Sir,

Thank you for the input.
How about TIG or MIG process? 

Any solution for such combination welding? 
Because the site project requirement is to join SS304 to Titanium grade 2.