Dear Experts,

  Could you advise us: For piping system hydrotests power plant project, we ave to prepare and use some temporary piping. The issue is :

- Is it Manadatory to perform NDE in related welds  and also PWhT
- For Flange fabrication, how to use plate thickness, any code or standard reference !

Please advise according your experience and with ASME reference .

Thank you.

--

Thanks and Regards, ?
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

Lakshman Kumar B

unread,
Dec 10, 2016, 12:28:16 AM12/10/16
to material...@googlegroups.com

Hi,

As per general practice,  temporary piping NDT & PWHT is not Mandatory – however for taking the decision so many if’s and But’s are their…

 

In one of my inspection days, piping material is of higher strength and with joint efficiency of 100% (due to 100% RT), but temporary piping is acquired by our local contractor and we also not monitored properly – neglecting that it is a temporary piping…

 

In the same HT, 6 failures are happen …

 

Failure 1.  - @25% HT Pressure – temp piping joints started leaking (welder used 7018 without baking and with lot of negligence – lot of porosity evident)

Failure 2. – @30 % HT Pressure – one more joint – identified defect is Lack of penetration and joint opened (can assume it’s a becomes a simple butt weld)

Failure 3 -  @40% HT pressure – tapping made for the instruments – fillet welding leak – SS nipple  to MS piping – no proper consumable used.

Failure 4 - @50% HT pressure  - Used asbestos gaskets given problem – changed to Neoprene rubber / EPDM

Failure 5 - @75% HT Pressure – few more joints started leaking – all are weld defects

Failure 6 - @ 85% HT Pressure – my seniors warned that the used MS piping can be busted at any time due to low “YS” and recalled the entire activity

 

Finally one more senior joined with me and guided me and trained me for the total issue – later on we had replaced the entire piping and with the proper WPS and all NDE measures implemented and successfully completed the test in one go….

So don’t take risk and each failure will cost u to repeat the entire test…

 

Final decision is with the client and contractor only – because NDE will incur some cost and time..

 

Also thickness of dummy – u can take reference of any code – as per ASME, IS or BS – anything is acceptable

 

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB15hqZTM7eP9EyGTUCdawvDKKHZxHHC%2BK5NhRbeOLt8YQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Shashank Vagal

unread,
Dec 10, 2016, 1:59:20 AM12/10/16
to material...@googlegroups.com, Nachiket Vagal, Samarth Vagal
Hello Zakaria,
Please see below
 
Best Regards,
Shashank C Vagal  (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, AERB)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel: +91 22 2611 6640 / (+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India   
www.neometalanalystndt.com / enq...@neometalanalystndt.com / nach...@yahoo.com



From: Zakaria ghrab <zakari...@gmail.com>
To: "material...@googlegroups.com" <material...@googlegroups.com>
Sent: Saturday, 10 December 2016 8:10 AM

Subject: [MW:25809] Temporary piping used in hydrotest - ASME B31.1
Dear Experts,

  Could you advise us: For piping system hydrotests power plant project, we ave to prepare and use some temporary piping. The issue is :

- Is it Manadatory to perform NDE in related welds  and also PWhT
NO FOR EITHER, 
BUT FOR PWHT - ANY WELDING INDUCED STRESSES IN EXCESS OF YS MAY BE UNDESIRABLE.
PERFORMING NDE ON ALL INCLUDING TEMPORARY MEMBERS WILL BE IN YOUR BEST INTEREST. IF A JOINT LEAKS BECAUSE OF ANY WELD DEFECTS, YOU WILL FACE EXTRA COST, ADDED TIME, RE-SCHEDULING, ETC  DUE TO  RE-HYDRO.
- For Flange fabrication, how to use plate thickness, any code or standard reference !
PLEASE SEE ATTACHED


Please advise according your experience and with ASME reference .

Thank you.

--

Thanks and Regards, ?
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
Blind flange thickness-.pdf

Zakaria ghrab

unread,
Dec 11, 2016, 10:08:44 PM12/11/16
to material...@googlegroups.com, Nachiket Vagal, Samarth Vagal
Thank you for sending.

Could you please inform for the reference for the table from code, standard.

Kind Regards.



2016-12-10 7:58 GMT+01:00 'Shashank Vagal' via Materials & Welding <material...@googlegroups.com>:
Hello Zakaria,
Please see below
 
Best Regards,
Shashank C Vagal  (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, AERB)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel: +91 22 2611 6640 / (+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India   

From: Zakaria ghrab <zakari...@gmail.com>
Sent: Saturday, 10 December 2016 8:10 AM
Subject: [MW:25809] Temporary piping used in hydrotest - ASME B31.1
Dear Experts,

  Could you advise us: For piping system hydrotests power plant project, we ave to prepare and use some temporary piping. The issue is :

- Is it Manadatory to perform NDE in related welds  and also PWhT
NO FOR EITHER, 
BUT FOR PWHT - ANY WELDING INDUCED STRESSES IN EXCESS OF YS MAY BE UNDESIRABLE.
PERFORMING NDE ON ALL INCLUDING TEMPORARY MEMBERS WILL BE IN YOUR BEST INTEREST. IF A JOINT LEAKS BECAUSE OF ANY WELD DEFECTS, YOU WILL FACE EXTRA COST, ADDED TIME, RE-SCHEDULING, ETC  DUE TO  RE-HYDRO.
- For Flange fabrication, how to use plate thickness, any code or standard reference !
PLEASE SEE ATTACHED


Please advise according your experience and with ASME reference .

Thank you.

--

Thanks and Regards, ?
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805

Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1461469163.207663.1481353081256%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages