Dear All,

1. Can anyone tell me what is the P.no for EN 10025 S275JR

    I searched in ASME IX but i didnt find.

2. I have WPS for CS (SA106) material, can i use this WPS for welding Mild steel (EN 10025 S275JR)

    looking for reply from u guys......

3. WPS shall be for only the material which they are going to weld and not to all equivalent material as mentioned in the Material specification description of WPS.

     is it correct????

shanmuganathan .subbiah

unread,
Apr 13, 2015, 1:36:42 AM4/13/15
to material...@googlegroups.com
Dear Naveen,

1.EN275JR is unassigned material as per SEC ix

2.No. to be prepared separate PQR 

3.yes

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a6e45df1-e3fb-4ddb-ad98-619f665411a5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--

Regards

SHANMUGANATHAN SUBBIAH
AIB- Vincotte International & Partners LLC

PO.Box-420, PC -116

MAF, Sultanate of Oman

Tel: +968 24565771

Fax: +968 24565772

Mob: +968 92096714

Web:www.vincotte.com

raouf salhi

unread,
Apr 13, 2015, 10:53:46 PM4/13/15
to material...@googlegroups.com
Dear sir ;

1 - The EN S275 JR is an europeen normalisation ( S mean structure , 275 is the yield strength , JR means 27 J at 20 °c for impact test) , the equivalent in ASME is the SA 572 ( p number 1).

2- they have the same P number but  A106 is a  pipe ( usually welded GTAW / SMAW) and the EN S275 JR is a plate usually welded only SMAW ( with backing ).
I don't think that you can use the same WPS.

3- no it's not correct

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258



Alagar Samy

unread,
Apr 14, 2015, 11:29:45 PM4/14/15
to material...@googlegroups.com
Dear Naveen,
 
                  As per Mr. Salhi said ,its correct that material equivalent.And Also i give the additional information

 

This is common carbon steel plate in S235JR, S235J0 and S235J2 steel grade. Heat analysis shall be used to determine the required chemical composition for carbon. Manganese, phosphorus, sulfur, silicon, and copper. Tensile strength, yield strength, and elongation shall be evaluated using tension test.

 

S symbol for structural steel 
275 indication of the min specified yield strength for thickness of under 16mm.
JR symbol 20 temperature impact test.
J0 symbol 0 temperature impact test

J2 symbol -20 temperature impact test

 

 

S275JR, S275J0 and S275j2 steel is a structural steel grade which be used in riveted, bolted, or welded construction of bridges and buildings.

 

For more information of S275j2 steel, please refer them in following.

 

The Chemical is max composition of product analysis:

 

Grade

C %

Si %

Mn %

P %

S %

N %

Cu %

S275J2

0.210

-

1.600

0.035

0.035

-

0.060

 

The mechanical properties steel plate

 

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

S275j2

8mm-100mm

275Mpa

430-560Mpa

21-23%

-20

27J

101mm-200mm

225-235Mpa

400-540Mpa

19%

-20

27J

201mm-400mm

215Mpa

380-540Mpa

18%

-20

27J

The min impact energy is longitudinal energy




2.You cant use same WPS,because this material plate type.You have WPS for pipe material.You can follow that WPS format as per your site using standard


Demir Alp

unread,
Apr 7, 2016, 4:09:30 AM4/7/16
to Materials & Welding
Dear Mr. Alagarsamy & Mr Salhi ;

Please correct me if i am wrong , but as per QW-211, a WPS qualified by pipe covers plate and vice versa.

Please see the extracted ASME Sec IX article in the attachment.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
...
qw-211.JPG

Chandra

unread,
Apr 7, 2016, 6:04:19 AM4/7/16
to material...@googlegroups.com
Dear Salhi,
EN S275JR material not listed in QW 422  
So, it was called as unassigned P.no

You have the WPS for A106Gr.B - you cant use for EN SA275JR material

You have to make a new PQR using the material EN S275JR

Pls refer to the para QW-424

Best Regards,
Chandra
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.
<qw-211.JPG>
Reply all
Reply to author
Forward
0 new messages