difference between fusion and penetration

434 views
Skip to first unread message

Rahul Chaudhari

unread,
Apr 3, 2015, 12:27:05 AM4/3/15
to material...@googlegroups.com
Dear Experts,

What is the difference between Fusion & penetration?
--
T

Kannayeram Gnanapandithan

unread,
Apr 3, 2015, 12:42:04 AM4/3/15
to materials-welding
basically same but if u can see with naked eye that is penetration (protrusion of weld metal at the root), fusion can not be seen with naked eye unless etched. 

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY

--
T

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V9ReVwjP8nwoUywJQofS0v6di66nrxq5MYApKUTAaYAxg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Biplab Pal

unread,
Apr 5, 2015, 3:16:20 AM4/5/15
to materials-welding
Dear Rahul,

Fusion: the process or result of joining two or more things together to form a single entity. the process of causing a material or object to melt with intense heat so as to join with another.

Penetration: the action or process of penetrating something.

This is the difference.


On Fri, Apr 3, 2015 at 7:35 AM, Rahul Chaudhari <navy...@gmail.com> wrote:
--
T

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V9ReVwjP8nwoUywJQofS0v6di66nrxq5MYApKUTAaYAxg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

meisam shokri arfaei

unread,
Apr 5, 2015, 5:15:02 AM4/5/15
to material...@googlegroups.com
If we search for the difference specially in the field of welding, it could be:

Some welding processes are categorized as fusion welding which we need melding during welding. In these processes we have fusion+penetration such as SMAW, SAW, ... .

In some other kinds of welding we have penetration without fusion such as friction welding (FW) or resistance welding (RW). We named these kinds of welding as solid state welding or non-fusion welding.

Regards


For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





sai jagadeesh MAVUDI

unread,
Apr 13, 2015, 10:55:44 PM4/13/15
to material...@googlegroups.com
Fusion means Two materials filler/electrode and parent metal should fuse or melt for good penetration.even there is good fusion some times those two not penetrate each other.


Thanks/Regards
Sai Jagadeesh Mavudi



--