G34CrMo4 hardness

25 views
Skip to first unread message

G.K.PILLAI

unread,
Jan 7, 2020, 5:49:08 AM1/7/20
to material...@googlegroups.com
dear experts,

can i have to know that maximam permissable hardness value for cast matrial G34CrMo4 , please provide if have any code reference for back up

Thanks&Regards,

G.K.PILLAI.

MOBILE

+97433329545    (QATAR)
+919500755882   (INDIA)

Raghuram Bathula

unread,
Jan 7, 2020, 6:11:48 AM1/7/20
to Materials-Welding
Std BS EN 10293 does not require hardness, any specific reason for this requirement?

J Prinsen

unread,
Jan 7, 2020, 6:13:35 AM1/7/20
to materials-welding
This material is NOT for code use, and only limited weldable.
Application shall be used only after proper testing of the welding procedure. (preheating 300-350 degrees centigrade, slow cooling) will offer you 400-500 HV,
PWHT at 600 degrees centigrade (if lower than the tempering temperature) will lower it to 300 - 350 HV 
Be carefull

Regards

Ir. Jurgen Prinsen (MSc/IWE)
Metalurgical and welding engineer/consultant

Van: "G.K.PILLAI" <pillai...@gmail.com>
Aan: "materials-welding" <material...@googlegroups.com>
Verzonden: Dinsdag 7 januari 2020 09:47:06
Onderwerp: [MW:30355] G34CrMo4 hardness

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACmDAmUh62iRRtPTzGE01E3WYB-b%2BQB%3Dn4eFF9jgdDoXbKYGOg%40mail.gmail.com.

G.K.PILLAI

unread,
Jan 7, 2020, 9:20:49 AM1/7/20
to material...@googlegroups.com
thanks for your reply


Thanks&Regards,

G.K.PILLAI.

MOBILE

+97433329545    (QATAR)
+919500755882   (INDIA)

G.K.PILLAI

unread,
Jan 7, 2020, 9:20:50 AM1/7/20
to material...@googlegroups.com
the supplier did some weld repair on the casting after tempering thatsway am seeking advice


Thanks&Regards,

G.K.PILLAI.

MOBILE

+97433329545    (QATAR)
+919500755882   (INDIA)
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.