combine 2 procedures in AWS D1.1

16 views
Skip to first unread message

Manoj John

unread,
May 14, 2015, 12:09:48 AM5/14/15
to material...@googlegroups.com
Dear Experts,

I have GTAW and SMAW procedure qualified seperately as per AWS D1.1.  Can we  prepare one WPS with these 2 qualified procedure as root run GTAW and subsequent run SMAW.

GTAW qualified in  8 mm thk  S 275 JR and SMAW qualified in 25 mm thk S 275 JR as per AWS D1.1

Thanks in advance.