Dear Experts,
I have GTAW and SMAW procedure qualified seperately as per AWS D1.1. Can we prepare one WPS with these 2 qualified procedure as root run GTAW and subsequent run SMAW.
GTAW qualified in 8 mm thk S 275 JR and SMAW qualified in 25 mm thk S 275 JR as per AWS D1.1