ASTM A262 Practice C - Acceptance criteria
161 views
Skip to first unread message
Chintan Raval
unread,
Jun 1, 2023, 10:49:20 PM
6/1/23
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Dear Expert,
For Austenitic stainless steel ( Type 304L, 316L) whats acceptance criteria for ASTM A 262 - Practice C as a recomanded practice.
Standard says it should be defined by user how ever client specification is silent in my case.
Thank you
james gerald
unread,
Jun 2, 2023, 5:15:32 AM
6/2/23
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
General acceptance standard for Material selection as below.
Thanks & Regards
J.Gerald Jayakumar
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com
.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAOdsS43jqObAzFfbmdTLSfEGXikYSJJ1O3E74F822dwV20TKjA%40mail.gmail.com
.
Adnan Ziad
unread,
Jun 2, 2023, 5:15:35 AM
6/2/23
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
In our project we follow practice E
Standard: ASTM A262 Practice E
(
Acceptance
criteria:
No
fissures or
cracking at 20X magnification)