Dear Raghuram Bathula,

   The main run pipe 20" is having thickness of 31.mm and being subjected to PWHT.
A dummy leg (12") is welded to the main pipe as dummy leg. pls confirm that, do we require PWHT at this joints as highlighted in below snap

image.png

Tajuddin Mohammed

non lue,
4 janv. 2020, 11:20:1104/01/2020
à material...@googlegroups.com
Yes we need to do the  PWHT of these type of joints as it is directly welded to the pipe

Mohammed Tajuddin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zOsMaca5bYCPWfVvRa1kRdBWqgcGKGMNEXf_k_dMXzMg%40mail.gmail.com.

Kannayeram Gnanapandithan

non lue,
5 janv. 2020, 03:28:1905/01/2020
à materials-welding
Governing thickness is as per B31.1 & 31.3 is Nominal material thickness??

pradip kumar Sil

non lue,
5 janv. 2020, 08:33:1905/01/2020
à materials-welding
If the material is CS as per B31.3, preheat temp is above 95 degree centrigrade then no need to conduct PWHT.
Only you have to qualify PQR

Mohd Siraj

non lue,
6 janv. 2020, 02:27:0606/01/2020
à Materials & Welding
No need.

But if pwht is service requirement you have to do.

MW

non lue,
7 janv. 2020, 00:19:4007/01/2020
à Materials & Welding
what is your code of construction, and service? any project specific requirements?

Venkadesh Lakshmanan

non lue,
7 janv. 2020, 03:24:5207/01/2020
à material...@googlegroups.com
No need, pls refer governing thickness specified in B31.3