Dear All,

We have a scenario where the SA335P91 - Weld joint had 3 repairs and PWHT Cycles.

Is there any code reference to limit the number of repairs / PWHT in the P91 weld joints or what permissible times PWHT could be done on the same joint.

In this case - Pipe MOC - SA335 P91 - NPS 4 and 13.89mm thick.

Thanks,
Sathish

Vishwas Keskar

unread,
Feb 15, 2022, 10:22:38 PM2/15/22
to material...@googlegroups.com
What is total holding time including repairs PWHT  and initial PWHT Holding time.

What was holding temperature?

Vishwas 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACOF__aYi2PepJFn6Or2ubuCp0wj5R4TE_vAbYTrQ64Y8dZo0g%40mail.gmail.com.

Mohd Siraj

unread,
Feb 15, 2022, 10:22:39 PM2/15/22
to Materials & Welding
sathish,

good workmanship and P91 one repair is considered.
 however, it depends on PQR, how many cycles are supporting it.

In our case, we did PQR with two repairs, one for construction and one for maintenance purposes.

james gerald

unread,
Feb 16, 2022, 12:53:33 AM2/16/22
to material...@googlegroups.com
Please see a snap shot below from API 938B about Repair.

Inline image


Thanks & Regards

J.Gerald Jayakumar




--

pradip kumar Sil

unread,
Feb 16, 2022, 10:22:11 PM2/16/22
to materials-welding
Hi Satish,

ASME code is silent regarding this issue. Better go for client specification.

Regards,
Pradip

George Dilintas

unread,
Feb 22, 2022, 11:00:20 PM2/22/22
to material...@googlegroups.com
and UW-38 in Section VIII-1



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

George Dilintas

unread,
Feb 22, 2022, 11:00:22 PM2/22/22
to material...@googlegroups.com
Check PW-40 in Section I of ASME, 