Regarding Weld area calculation for branch reinforcement as per ASME B 31.3

273 views
Skip to first unread message

atul khatri

unread,
Jul 16, 2019, 1:52:18 AM7/16/19
to material...@googlegroups.com
Hello experts,
As per clause 304.3.3 of ASME B 31.3 (Reinforcement of welded branch connections), Area A4 is the area of other metal provided by welds and properly attached reinforcement.

While calculating the weld area , the minimum value of tc=0.7 Tb or 6mm (1/4 in.) ,except that larger dimensions may be used if the welder has been specifically instructed to make the welds to those dimensions.

image.png

Now my query is -- 
In case if welder has gone with higher weld thickness and weld throat is coming more than 6mm, than the weld area for reinforcement should be calculated based on higher thickness or restricted to 6mm only ?

Thanks and regards
Atul Khatri

atul khatri

unread,
Jul 16, 2019, 2:31:47 AM7/16/19
to material...@googlegroups.com

In addition to my previous email, I would like to make my query more clear ..
1.  If actual weld throat thickness is higher than the minimum specified in code , should we take the benefit of the extra weld area in calculation of reinforcement area ?
2. Does the extra heat input due to additional weld may distort the base metal and also affect the mechanical properties of weld ,HAZ and base metal ?

Vinay Thattey

unread,
Jul 16, 2019, 11:19:41 PM7/16/19
to material...@googlegroups.com
Restrict to specified thickness while carrying out calculations.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeDck91TCVhuBVvm%2Bn3wsE5i%3Dhsc9yP3rB1-LCnMG2bVcA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

George Dilintas

unread,
Jul 17, 2019, 12:24:08 PM7/17/19
to material...@googlegroups.com
usually not, unless you really mesh up in the welding

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

George Dilintas

unread,
Jul 17, 2019, 12:24:08 PM7/17/19
to material...@googlegroups.com
No, the calculations have to be based on the minimum fillet weld size given by the code

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.

atul khatri

unread,
Jul 18, 2019, 4:13:34 AM7/18/19
to material...@googlegroups.com
I tried in PV Elite  software for shell to nozzle reinforcement calculation and there by increasing the fillet weld leg beyond the code limits , the reinforcement area got increases . So here the software results were opposite to what you recommended. 
Please advise. 