Hi,
It’s allowed by Sec VIII, DIV1. Please see the highlighted clauses as below.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent Welding & Metallurgical Engineering Specialist
Saudi Aramco Approved Designated Project Welding Engineer (DPWR)
Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
UW-40 PROCEDURES FOR POSTWELD HEAT TREATMENT:

From: vishal hirde <vishalh...@gmail.com>
Sent: June 25, 2022 8:24 AM
To: material...@googlegroups.com
Subject: PWHT Segment Wise for 9 Meter Dia Vessel
Dear All,
We are fabricating a Vessel of Diameter 9 Meter at Site, requires PWHT: Material Grade SA 516 Gr. 70.
For Circumferential Joint PWHT can it be performed Segment Wise as diameter is more??
Pl. Confirm as per ASME Sec VIII Div 1 can it be done in Segment Wise.
--
With Best Regards,
Vishal Hirde
Thanks & Regards
J.Gerald Jayakumar
Thanks & Regards
J.Gerald Jayakumar
Thanks & Regards
J.Gerald Jayakumar
Thanks & Regards
J.Gerald Jayakumar
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2053801785.4862984.1656227327732%40mail.yahoo.com.
---