ASTM A 578 LEVEL B

316 views
Skip to first unread message

Ali Asghari

unread,
Feb 2, 2015, 4:39:54 AM2/2/15
to material...@googlegroups.com
Dear All
In lamination check by straight probe , some lamination and inclusion detected but they have a echo height less that 15%. Acceptance of project is level B of ASTM A578.
Now  I want to know in 8.2 of A578 , small discontinuities must have total loss of back reflection or not?
Grade of material is API 2H GR 50 Z.
Regards.

meisam shokri arfaei

unread,
Feb 3, 2015, 3:53:12 AM2/3/15
to material...@googlegroups.com
Dear Ali,

8.2 refers you to the discontinuities which pass 8.1 requirements for loss in back reflection and then discuss about the size of such discontinuities.

Regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALcH7WBi%2B9cYffHt97RTS2ZnwCocUaB2oNywJP%2BVC53ZCN8Yng%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





george....@gr.bureauveritas.com

unread,
Feb 3, 2015, 4:28:53 AM2/3/15
to material...@googlegroups.com

It is not so simple as you describe it. It is a combination of total loss of back reflection with continuous indications.
Read 8.1 carefully and make a sketch of your indications

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Ali Asghari ---02/02/2015 11:39:57---Dear All In lamination check by straight probe , some laminationAli Asghari ---02/02/2015 11:39:57---Dear All In lamination check by straight probe , some lamination and inclusion

--

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to


To post to this group, send email to


To view this discussion on the web visit

Ali Asghari

unread,
Feb 4, 2015, 5:43:26 AM2/4/15
to material...@googlegroups.com
Dear Meisam.
Thank you for responding.
I want to know 8.2 applicable for small discontinuity that has a TOTAL loss back reflection or loss back reflection?
Regards. 

meisam shokri arfaei

unread,
Feb 4, 2015, 7:17:19 AM2/4/15
to material...@googlegroups.com
Dear Ali,

There is no need to use total loss of back reflection. Actually this is not practical to calculate total loss of back reflection for discontinuities which you could see the full height of back reflection between them.
Consider a situation in which you fount 3-4 indications, each one produce a loss in back reflection, but when you move the transducer between them you could see the full height of back reflection. If the distance between those discontinuities is smaller than the size of the largest discontinuity, this will be unacceptable situation.

If you need more, feel free to call my mobile.

Regards