Hi Meisam,
You need to trust on the certification provided by the consumable manufacturer. Typically all reputed SAW welding consumable manufacturers carry out wire flux classification test, along with which they need to carry out the test for diffusible hydrogen content also.
Look at ASME Sec II, Pt C-SFA 5.17 for typical guidelines( I find this to be better explained)
AWS standard for diffusible hydrogen content is: (AWS A4.3-93-2006),. Standard Methods for Determination of Diffusible Hydrogen Content of Martensitic, Bainitic, and Ferritic Steel Weld Metal . This process is quite tedious. Only knowledgeable labs who test welding consumables on a regular basis, are capable of doing. One needs to find out more details before proceeding with the welded samples.
Hope this clarifies your doubt. Read through the following document for more details.
Thanks
Pradip Goswami, P.Eng,IWE
Welding &
Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email
to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMts2uhtD4ToPUH1D9QZWnOvaCfubxj_SugMdmVZtoKmnBA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Hi Meisam,
You need to trust on the certification provided by the consumable manufacturer. Typically all reputed SAW welding consumable manufacturers carry out wire flux classification test, along with which they need to carry out the test for diffusible hydrogen content also.
Look at ASME Sec II, Pt C-SFA 5.17 for typical guidelines( I find this to be better explained)
AWS standard for diffusible hydrogen content is: (AWS A4.3-93-2006),. Standard Methods for Determination of Diffusible Hydrogen Content of Martensitic, Bainitic, and Ferritic Steel Weld Metal . This process is quite tedious. Only knowledgeable labs who test welding consumables on a regular basis, are capable of doing. One needs to find out more details before proceeding with the welded samples.
Hope this clarifies your doubt. Read through the following document for more details.
Thanks
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of meisam shokri arfaei
Sent: Sunday, September 11, 2016 3:47 AM
To: materials-welding@googlegroups.com
Subject: [MW:25367] SAW flux with low hydrogen content
Dear Experts
I need some information about standard method or test procedure which introduce testing on SAW flux to assure low hydrogen content.
For example when I have BS EN ISO 14174 / S A FB 1 65 AC H5 flux, How could I assure this is H5?
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMts2uhtD4ToPUH1D9QZWnOvaCfubxj_SugMdmVZtoKmnBA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAEVn8ssFyzRHqLl%2BdNQTVrEBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.