Can any one tell me about selection fo welding consumables for 42CrMo4 material with E250 BR 

Parminder Singh

unread,
Oct 16, 2023, 3:22:24 AM10/16/23
to material...@googlegroups.com
GTAW ER 90S-B3 
SMAW E 11070 

On Fri, Oct 13, 2023, 22:30 SANJAY SINGH <sanjay.k...@gmail.com> wrote:
Can any one tell me about selection fo welding consumables for 42CrMo4 material with E250 BR 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4205fd8d-e84f-4655-a2f2-1a8eb59dee97n%40googlegroups.com.

Ritesh Kumar Singh

unread,
Oct 16, 2023, 3:45:22 AM10/16/23
to material...@googlegroups.com
Dear Sir,
I thought Er90S-B3  is used for low alloy 

Parminder Singh

unread,
Oct 24, 2023, 9:12:36 AM10/24/23
to material...@googlegroups.com

42CrMo4 material is equivalent to ASTM 4140. 