Dear Experts 

X22 CRMOV12-1 +QT2 what is the requirements of mentioned welding and consumable please advised.

Waris Ali 

navnitkumar parikh

unread,
Apr 26, 2020, 1:03:36 AM4/26/20
to material...@googlegroups.com
Dear Mr.Ali,

Refer attached welding consumable catalogue. It will  give some reference for welding of X22CrMoV12-1.

Navnitkumar Parikh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC23Ko3OAgNEhgd3CYR7A3EKw4aND_T-de5oBNcp7bf7L-exDA%40mail.gmail.com.

Pradip Goswami

unread,
Apr 26, 2020, 11:21:29 PM4/26/20
to Materials & Welding
X-20 is a nasty steel, just ideas about welding welding consumables, methods would not help. If you have mastered the welding methods and techniques for Grade-91 steel, then handling X-20 would be easy, although this steel is always problematic.
I had handled this steel 30+ years ago for a major power plant project. If you're interested , feel to contact me offline or in LinkedIn.