To the best of my knowledge, it is not prohibited to weld a pad or a saddle on a weld.
You may check in chapter 382.5 and more particularly in 328.5.4.
Check 341.3.1 for inspection requirements
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Hafiz Ali Alvi ---14/07/2015 07:00:19---Deal All, I have a question about Overlapping of RF Pad With an Existing Weld Joint.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/COL402-EAS147FEC1E05A2795171B521DE79C0%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.
[attachment "image2.PNG" deleted by George H Dilintas/GRC/VERITAS]
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/COL402-EAS147FEC1E05A2795171B521DE79C0%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.
[attachment "image1.PNG" deleted by George H Dilintas/GRC/VERITAS]
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/COL402-EAS147FEC1E05A2795171B521DE79C0%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information.
To know more, please click on the following link: http://disclaimer.bureauveritas.com
| As per site condition you can accept it. But before welding please be sure that the haz of rf pad and joint are apart from each other. |
|
|
|
|
|
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1436877467.4386.YahooMailAndroidMobile%40web181301.mail.ne1.yahoo.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/COL402-EAS244AF778E187ADCC0F9684AE79B0%40phx.gbl.