Can the certificate type 3.1 re-certified by 3rd party inspection?

260 views
Skip to first unread message

Hyunjong Moon

unread,
Jun 19, 2015, 11:05:32 AM6/19/15
to material...@googlegroups.com
Dear. All.
I would like to know whether the piep can be re-certified as type 3.2 with certificate issued by independence agency.
 
When the 3.2 certificate type is requested the manufacturing, however, mill(Pipe) has already prepared a 3.1 type and delivered document/material to plant manufacturer.

In this case, I’d like to know that plant manufacturer can use this pipe?

Of cause never use.

 

Normally, whenever we met above case, we have tested the mechanical properties, chemical composition and special requirement for this project under 3 party’s witness. (LR, TUV & SGS)

And then, we can receive the certificate type 3.2 issued by witnessed inspection agency.(LR, TUV & SGS)

Actually, I have been maintaining the certificate 3.2 type for above situation and the certi. has been issued by TUV.

 

However, someone told me that upgrading the certificate from 3.1 to 3.2 type never do, although the tests have been carried out under 3 party’s witness after delivered from Mill Maker.

They are insisting that the certificate is only 3.1type + witness the test by 3party.

 

Because of following context,

3.2 type is document prepared by both MFG and 3rd party agency.

 

Please let me know that in this case, the 3.2 type certificate can be issued by 3 party agency or not?

 

4.2 Inspection certificate 3.2 “type 3.2”

Document prepared by both the manufacturer’s authorized inspection representative, independent of the manufacturing department and either the purchaser’s authorized inspection representative or the inspector designated by the official regulations and in which they declare that the products supplied are in compliance with the requirements of the order and in which test results are supplied.

gprak...@gmail.com

unread,
Jun 19, 2015, 11:32:44 AM6/19/15
to Hyunjong Moon
It is witnessed by either manufacturer's representative or purchaser's representative. The tests witnessed are mentioned in 3.2. All other parameters are in 3.1. So both have to be seen together. If manufacturer,s rep is stationed in mill they can issue 3.2 with all parameters.

Rgds
 Prakash. G. 
ASME AIS
Independent Consultant. ASME/ISO/PED
From: Hyunjong Moon
Sent: Friday, 19 June 2015 19:05
Subject: [MW:23094] Can the certificate type 3.1 re-certified by 3rd party inspection?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/34b16016-6a0a-4c96-8490-c50e8c312198%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

savad qac

unread,
Jun 20, 2015, 12:31:57 AM6/20/15
to material...@googlegroups.com
Dear,

The up gradating ( Heat number) shall be through endorsing the  3.1 certificate by an Independent agency with the witness/concurrence of the buyer/user. The test shall be minimum as listed in MTC.
3.1 endorsed by an Independent inspection agency is equivalent to 3.2.

Regards
Savad

On Fri, Jun 19, 2015 at 10:11 AM, Hyunjong Moon <zzong...@gmail.com> wrote:
Dear. All.
I would like to know whether the piep can be re-certified as type 3.2 with certificate issued by independence agency.
 
When the 3.2 certificate type is requested the manufacturing, however, mill(Pipe) has already prepared a 3.1 type and delivered document/material to plant manufacturer.

In this case, I’d like to know that plant manufacturer can use this pipe?

Of cause never use.

 

Normally, whenever we met above case, we have tested the mechanical properties, chemical composition and special requirement for this project under 3 party’s witness. (LR, TUV & SGS)

And then, we can receive the certificate type 3.2 issued by witnessed inspection agency.(LR, TUV & SGS)

Actually, I have been maintaining the certificate 3.2 type for above situation and the certi. has been issued by TUV.

 

However, someone told me that upgrading the certificate from 3.1 to 3.2 type never do, although the tests have been carried out under 3 party’s witness after delivered from Mill Maker.

They are insisting that the certificate is only 3.1type + witness the test by 3party.

 

Because of following context,

3.2 type is document prepared by both MFG and 3rd party agency.

 

Please let me know that in this case, the 3.2 type certificate can be issued by 3 party agency or not?

 

4.2 Inspection certificate 3.2 “type 3.2”

Document prepared by both the manufacturer’s authorized inspection representative, independent of the manufacturing department and either the purchaser’s authorized inspection representative or the inspector designated by the official regulations and in which they declare that the products supplied are in compliance with the requirements of the order and in which test results are supplied.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/34b16016-6a0a-4c96-8490-c50e8c312198%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Withe Best regards

Savad Salahudeen