Allowable Tube Wall Reduction Tube-to-Tubesheet Joints expended in 2 grooves and seal welded

84 views
Skip to first unread message

Pushpraj Anand

unread,
Nov 15, 2015, 11:54:08 PM11/15/15
to materials-welding
Dear experts
 Please let me know the Allowable Tube Wall Reduction Tube-to-Tubesheet Joints expended in 2 grooves and seal welded 

Tube is SA179 ,20 mm OD & 2 mm thick
Tube sheet SA299 Gr B , 20.20 +_ 0.05 mm hole dia with 2 grooves inside the hole 

Please also share the applicable clause of TEMA or ASME stand.

Regards
Pushpraj Anand
  

Madhan S

unread,
Nov 16, 2015, 11:49:52 PM11/16/15
to Materials & Welding
Dear Pushpraj

Formula for tube expansion, D=d+e+t

D- Tube ID after expansion.
d- Tube ID before expansion.
e- Clearance between tube OD and Plate ID
t- Applied Diameter expansion is 0.6 mm. (0..6mm Use can change depending on your groove depth.)

In your case you have seal welding also. So Don't worry for leakage.

With Regards,
Madhan. S

CHINTUKUMAR GANDHI

unread,
Nov 28, 2015, 3:10:08 AM11/28/15
to material...@googlegroups.com
Dear Mr. Pushpraj,

Since ASME & TEMA does not specifiy tube wall thickness reduction limit, for C.S. materials 8-10% thinning is recommended as per Good Engg. Practice and reputed PMC spec.

Thanks & regards,

C. R. GANDHI


From: Madhan S <madha...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Tuesday, November 17, 2015 9:11 AM
Subject: [MW:23889] Re: Allowable Tube Wall Reduction Tube-to-Tubesheet Joints expended in 2 grooves and seal welded

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/80f9e288-02b6-4df8-beab-762d5de20648%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages