What’s the design and fabrication code for Piping??
Usually pressure piping have to be hydro tested (by default) as like pressure vessel. No exceptions to rules?
A citation from the appropriate code or mentioning the appropriate code would be appreciated.
Thanks.
P.Goswami.P.Eng, IWE.
Welding&Metallurgical Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1216733524.5643000.1490782373350%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAB/s9XS594ZCoMHlmX4xaZ3CgAAAEAAAADNg4iY9mnhIoxuiarCDI9UBAAAAAA%3D%3D%40quickclic.net.
What’s the design and fabrication code for Piping??
Usually pressure piping have to be hydro tested (by default) as like pressure vessel. No exceptions to rules?
A citation from the appropriate code or mentioning the appropriate code would be appreciated.
Thanks.
P.Goswami.P.Eng, IWE.
Welding&Metallurgical Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
From: 'Ganesan' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: March 29, 2017 6:13 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26313] Hydro Test
Dear Experts,
Could you please share the standard requirements for piping hydro test, because our chines contractor has not ready to conduct hydro test for the same piping. they said as per chines standard no need hydro test.
Thanks & Regards, K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1216733524.5643000.1490782373350%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAB/s9XS594ZCoMHlmX4xaZ3CgAAAEAAAADNg4iY9mnhIoxuiarCDI9UBAAAAAA%3D%3D%40quickclic.net.
Pneumatic test is not advisable for safety and integrity of piping components. Hence Hydro test is the default choice.
Hope it clarifies your doubt.
Thanks.
P.Goswami.P.Eng, IWE.
Welding & Metallurgical Engineering Specialist
This email has been checked for viruses by AVG antivirus software.
www.avg.com