Hi,

Can anyone share a info. about 900RTJ AND 1500RTJ?

Can we use 900 RTJ FLAN for upto 3”?  I can see in piping spec that upto 2” is 1500 and above 2” is 900# and material is same.  Is there any difference between construction of 900# and 1500# rating RTJ flanges?

 

Thanks in advance J
sri

Enayat Zarei

unread,
Nov 6, 2015, 6:42:48 AM11/6/15
to material...@googlegroups.com
Dear Sri,

Please refer to relevant of ASME B16.5 that is attached.

Best Regards,
Zarei


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/214feee3-3361-40a1-97ce-fdef96f0d50f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

B16.5.png
Reply all
Reply to author
Forward
0 new messages