Acceptance criteria for wrinkles

80 views
Skip to first unread message

raj kumar

unread,
Jan 15, 2025, 11:59:45 PM1/15/25
to material...@googlegroups.com
Pls suggest what is acceptance criteria for wrinkles on Stainless steel elbow.


Kannayeram Gnanapandithan

unread,
Jan 16, 2025, 12:32:21 AM1/16/25
to material...@googlegroups.com
pl ref BS EN 12952-5

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Jan 16, 2025 at 10:29 AM raj kumar <srajme...@gmail.com> wrote:
Pls suggest what is acceptance criteria for wrinkles on Stainless steel elbow.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CABHGzEUoZU9Gk%3DQmNv3Tcm2VW3znE-X%2B%3DLUjbPaz%3D4irh9t8tg%40mail.gmail.com.

shri krishna tripathi

unread,
Jan 16, 2025, 1:01:37 AM1/16/25
to material...@googlegroups.com
Pls see PFI ES 24



--
Shri Krishna Tripathi
IGCAR,
Department of Atomic Energy

Raviraj Gohil

unread,
Jan 16, 2025, 5:10:46 AM1/16/25
to material...@googlegroups.com

Please refer ASME SEC II PART A, SA/A 403 clause no. 10

Mechanical marks deeper than 1.6 mm shall be removed and subjected to maintain thickness