Hello ;

We work for welding activity pipeline 12”         X52       thickness 8.38 mm

Root / hot pass      GTAW

Filling / cap            SMAW

In order to optimize production Contractor propose to proceed with GTAW  first ,   for example for he weld  first 10 weld joint GTAW  after that he come back tomorrow  with and filling and cap  weld joint with SMAW.

 

It’s some issue for that    ?

udaya bhaskar

unread,
Oct 22, 2020, 10:55:03 AM10/22/20
to material...@googlegroups.com
Hi,

There is no issue here, Root & Hot passes are essential variables at piping.
You can do.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/386e7357-4115-479b-b8bf-45df08b78becn%40googlegroups.com.


--
With Regards

Udaya bahaskar.D

Kannayeram Gnanapandithan

unread,
Oct 22, 2020, 10:56:54 AM10/22/20
to materials-welding
check api 1104, time laps are important if you have specified in WPS

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--

Nadakuditi kiran kumar

unread,
Oct 23, 2020, 12:03:37 AM10/23/20
to material...@googlegroups.com
Dear Sir, Check your WPS whether it is single heat cycle or 60% of the thickness to be weld before welding going to stop, in our project min 60% to be weld shall be completed.
Thanks & Regards

srinu p

unread,
Oct 23, 2020, 12:03:37 AM10/23/20
to material...@googlegroups.com
Hi,

There is no problem, need  to do atleast  half thickness or hot pass which ever is greater before removing the clamp/before interruption of weld.

--