PQR for stainless steel with Duplex stainless steel

116 views
Skip to first unread message

mohammed hashif pattambi

unread,
Mar 9, 2023, 4:09:40 AM3/9/23
to Materials & Welding
Gents,

during PQR for WPS of SS to DSS using filler Er Ni Cr MO-10, Corrosion test is failing. can i get any advise and suggestion on this.

Vishwas Keskar Welding Manager WELDING

unread,
Mar 9, 2023, 4:35:42 AM3/9/23
to Materials & Welding

Pl. furnish details as a minimum .
1)Which corrosion test ?
2)Welding process?
3)What brand of consumables ?
4)Heat input while welding?
5)Which DSS steel - 32205 ?
Pl. send in detail information then the correction/suggestion can be given 

Thanks and regards

Vishwas -IWE

Mubashir khan

unread,
Mar 9, 2023, 4:35:56 AM3/9/23
to material...@googlegroups.com
In our project Er2590 they are using for duplex

On Thu, Mar 9, 2023, 12:09 PM mohammed hashif pattambi <mohammed...@gmail.com> wrote:
Gents,

during PQR for WPS of SS to DSS using filler Er Ni Cr MO-10, Corrosion test is failing. can i get any advise and suggestion on this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/099b14b7-c726-47f7-a62a-5466c81ff2acn%40googlegroups.com.

Sudhakar Kuppuswamy

unread,
Mar 12, 2023, 8:22:52 AM3/12/23
to material...@googlegroups.com

Keep other parameters and details aside, it is presumed that you would have performed ASTM G48 Method A. 

If your answer is Yes. Certainly, the ASTM G48 Method A will keep failing for SS#DSS combination. 

Please share other details as requested below.

Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhak...@gmail.com.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Pham Thanh Tinh

unread,
Mar 13, 2023, 12:49:55 AM3/13/23
to material...@googlegroups.com
Sir.

1. What Group of SS and DSS?
2. Welding process? 
3. What method did you use for the Corrosion test?
4. Temperature: your client requirement for a test?
5. Heat input while welding, Interpass temperature?
6. What type of Argon is used for Purging Gas and shielding?
7. Branch of welding consumable. 
8. What type of chemical is used for pickling and passivation? 

Please reference API 582 for correctly chosen welding consumable as per your base metal and design as per project specification requirement. 

Vào Th 5, 9 thg 3, 2023 vào lúc 12:09 mohammed hashif pattambi <mohammed...@gmail.com> đã viết:
Gents,

during PQR for WPS of SS to DSS using filler Er Ni Cr MO-10, Corrosion test is failing. can i get any advise and suggestion on this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


Reply all
Reply to author
Forward
0 new messages