Dear Experts,
The PQR is qualified on as per ASME SEC IX and ASME B31.3 requirement & . Thickness criteria is to followed as per ASME B31.3:
P. No. 1 GR.1 (A106 Gr.B) to P. No. 1 Gr.2 (A105N),
Impact @ -20 Deg C as per project specification requirement
Thickness for WPS 1.5 mm to 20 (T to 2T) mm or 5 to 16 mm (T/2 to T+6).
Kindly give the code reference:
Thanks & Regards,
Mohd. Azam
Τ/2 to T + 6 (see table 323.3.1)
you will never find impact test qualification requirements and ranges in Section IX. Always in the construction Code Section
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Mohd Azam ---22/01/2015 13:30:46---Dear Experts, The PQR is qualified on as per ASME SEC IX and ASME B31.3 requirement & .
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXS46ip-dH%3Dg2d0P_AyhtA4PaWkVNavRCUT0YH%3DAWoGs0g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFA9B1FC5D.6C8AB053-ONC2257DD5.004374EE-C2257DD5.004395F0%40LocalDomain.