Regarding requalification of Procedure qualification required or not for when welding FCAW filler wire brand name change

27 views
Skip to first unread message

G.S. PERUMAL

unread,
Jul 13, 2025, 10:26:06 PMJul 13
to Materials & Welding
We have having WPS with impact test at -29 Deg.c for FCAW process. as per ASME SEC-IX. As per engineering  requirement Impact test required at -29Deg.c.
Now new filler wire brought having same SFA NO but different brand name from same manufacturer. Mechanical properties were same. Impact test carried out at -40 Deg.c as per MTC.
We need to qualify new PQR or Proceed with existing PQR.

Regards,
Shanmuga.

bavithran samuthralingam

unread,
Jul 14, 2025, 10:31:18 PMJul 14
to material...@googlegroups.com
According to ASME Section IX, if the new filler wire has the same SFA number but a different brand name from the same manufacturer, and the mechanical properties are the same, you might not need to requalify the PQR.

However, since the impact test was carried out at -40°C, which is more stringent than the required -29°C, and the results are satisfactory

Get approval from the Client  to use the new filler wire with the existing PQR.





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/97c89848-d5c1-4b58-ab03-66536ddb850an%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages