For DSS: Same above range as a base and to meet IQI.
Penetration level: As per ASME sec. V
For CS: No Specific limits. X-ray energy and technique to achieve required penetration and IQI sensitivity up to job thickness.
For DSS: Same above and to meet IQI for the thickness used.
Sridhar.
----------------------------------------------------------------------------------------------------------------------------------------------------------------------
--