Dear All,

   In site we have one case that pipe shoe support weld clash with elbow weld, i.e.gap between weld toes is zero.

   Can we proceed with the joints at least 100mm of each welds will be tested with 100% X-ray, 100% VT and 100% MT

George Dilintas

unread,
May 21, 2019, 5:34:17 AM5/21/19
to material...@googlegroups.com
what is the applicable Code/ Standard (B31.1?, B31.3? other?)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8bd4bdfa-027b-44c6-96d8-b5bcee41de95%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Chiranjeevi A

unread,
May 22, 2019, 5:10:13 AM5/22/19
to material...@googlegroups.com
Dear George,

We are using ASME B31. 3

Mohamed Muneeb

unread,
May 23, 2019, 7:44:46 AM5/23/19
to materials-welding
Hi,

To contemplate on your scenario, after the butt weld of pipe to elbow, your construction team proceeded welding the shoe on elbow ? So as per your statement it is not just kissing with haz but clashing, which means your construction did intentionally, now you're here for correction.

Yes correction can be done as per your above proposal if your company has any standard stating with the clause or if you have a procedure or write and take approval.

One of world's top company standards clause waives your requirement with what you have proposed.

Check SAES-W-011, search for encroachment.

Thanks 

Muneeb

pradip kumar Sil

unread,
May 24, 2019, 2:26:14 AM5/24/19
to materials-welding
Code is silent regarding minimum distance between the weld. Different project has mentioned different criteria.Pls go through your project specification otherwise take a approval from client.

Bhima Kanjariya

unread,
May 24, 2019, 2:26:14 AM5/24/19
to Materials & Welding
dear Anil,
first of tell that with type of support is there. is it trunnion support, angle support etc.

if trunnion support is there then you can proceed with your weld and followed by NDT
you can proceed with the weld but take care while welding that there should be gap in welding of support whenever it collide with elbow weld.

don't weld on elbow weld. skip the welding on elbow weld. other place proceed with joint and do the NDT.

Thanks