Heating /cooling rate in PWHT

432 views
Skip to first unread message

pradip kumar Sil

unread,
May 7, 2015, 1:39:18 AM5/7/15
to materials-welding
Dear All,
Can anybody inform me,  Piping PWHT  heating & cooling rate where i will get in B-31.1/B31.3.
Thanks & Regards
Pradip

pradip kumar Sil

unread,
May 7, 2015, 5:42:23 AM5/7/15
to materials-welding
 B-31.1 PARA 132.5 it is mentioned PWHT Heating & Cooling requirement.

Above 600F( 315 degree centrigrade ), the rate of heating & cooling shall not exceed 600 degree Fahrenheit/Hr ( 315 degree centrigrade/hour) divided by one half the maximum thickness of material in inchat weld, but in no case shall the rate exceed 600 degree fahrenheit/hr ( 325 degrre centrigrade/hour )

My question is how i will calculate, if in case 36mm thickness in carbon steel as well as 36 mm thickness in P-91 material
BR
Pradip

---------- Forwarded message ----------
From: <hwj...@tce.co.in>
Date: Thu, May 7, 2015 at 1:12 AM
Subject: Re: [MW:23221] Heating /cooling rate in PWHT
To: prad...@gmail.com
Cc: materials-welding <material...@googlegroups.com>



It is available .Refer chapter of fabrication, assembly and erection ,in it.







your truly
H W JOSHI
ENGINEER MECHANICAL
TATA CONSULTING ENGINEERS LTD
MUMBAI - 400 083
TEL : 022 61148414



pradip kumar Sil <prad...@gmail.com>
Sent by: material...@googlegroups.com

07-05-2015 11:11


To
materials-welding <material...@googlegroups.com>
cc
Subject
[MW:23221] Heating /cooling rate in PWHT


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8mhqLmJYk0%2BDTuC3zCB-6vTCJ6wmzkuy7NShyQP2capLA%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------


Reply all
Reply to author
Forward
0 new messages