Dear Experts,
Good morning!
Has anyone performed ferrite–austenite phase evaluation for Duplex Stainless Steel (DSS)?
As per my understanding, this requirement has been incorporated in ASME Section IX under Non-Mandatory Appendix M (M-600). I would appreciate if you could share your experience, procedures followed, or any practical challenges faced during implementation.
Whether we can do with any machines without help of labratories
Looking forward to your valuable inputs.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2W4yRfBs9N1zWWFd6EfNApA8u7-dqMYgr0HsXCkEDJVhA%40mail.gmail.com.

--
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kMeTF2tZsULqy7mnWVNh5mwqPYZK9AZTgL%3DEGuu36UTA%40mail.gmail.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kMeTF2tZsULqy7mnWVNh5mwqPYZK9AZTgL%3DEGuu36UTA%40mail.gmail.com.
This requirement is not applicable to PQR; it is applicable to WPQR.
For WPQR, can we measure the ferrite content using a ferritoscope during production in the shop, instead of performing the point count method?
Regards,
Nambirajan A