How much welding to be finished

43 views
Skip to first unread message

pradip kumar Sil

unread,
Feb 22, 2016, 5:50:53 AM2/22/16
to materials-welding
Dear All,
Welding can be stopped ( Carbon Steel Material )How much percentage of welding finished.
I remember 33% to be completed at a time with non removal of slag.
Can anybody guide me to provide code reference.
Regards,
 

Kannayeram Gnanapandithan

unread,
Feb 22, 2016, 8:45:20 AM2/22/16
to materials-welding

Carbon steel is not a problem, but alloy steel or high strength steel, minimum 6mm or 1/3 of thick before stopping welding

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3Dgp93tNBfryb%3D3Ar56eM60i%3DB0wk3mxm_z5KbZBiRy%3Dw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages