I would suggest to read and understand the chapter 2.5.3 of National Board Inspection Code - repairs and alterations
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
pradip kumar Sil ---23/06/2015 08:31:19---Dear All, Post weld hydrogen bake out ( Post weld baking ) is aplicable for ASTM 335
From: pradip kumar Sil <prad...@gmail.com>
To: materials-welding <material...@googlegroups.com>
Date: 23/06/2015 08:31
Subject: [MW:23103] Post Weld Hydrogen bake out...Post weld baking -P-22
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
To post to this group, send email to
material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DCaX1AdqLcBxo0Ni8xeX8EnyQZ7tq8zv6eOE9Ovf7hXQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/561924799.3748955.1435041510885.JavaMail.yahoo%40mail.yahoo.com.