ASME P number for EEMUA 144

55 views
Skip to first unread message

thulaib arakkal

unread,
Mar 17, 2024, 3:48:13 AM3/17/24
to material...@googlegroups.com
Dear All,

Can we assign P number 34 to EEMUA 144 UNSC7060X 90/10 CuNi.

Regards,

Thulaib

Vinay

unread,
Mar 17, 2024, 4:26:28 AM3/17/24
to material...@googlegroups.com
in my view , YES

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JPwAzTU2hUC49U59gO7%2BqkMtNEv75S8LadfwyAcr94AVQ%40mail.gmail.com.

RIJU PATHROSE

unread,
Mar 17, 2024, 4:26:28 AM3/17/24
to material...@googlegroups.com

No, shall be assigned as UNLISTED material EEMUA 144 UNSC7060X 90/10 CuNi. which is not assigned in ASME Sec IX. 
Therefore the subject welding procedure cannot be qualified for material P34 as per Sec IX clause 403.11, which is an essential variable.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JPwAzTU2hUC49U59gO7%2BqkMtNEv75S8LadfwyAcr94AVQ%40mail.gmail.com.


--
Best Regards,
Riju pathrose
QA/QC Engineer
Mob: +966534148879
Reply all
Reply to author
Forward
0 new messages