Would 317L grade stainless instead against 316L

18 views
Skip to first unread message

Harikrishna Desiti

unread,
Sep 13, 2016, 7:29:08 AM9/13/16
to material...@googlegroups.com
Dear sir / experts, 
                          
We are now at the stage of selection of some analyzers,Would i used 317L grade stainless instead against 316L grade stainless. 


Thanks & Regards..........?

HARIKRUSHNA DESITI

pgoswami

unread,
Sep 13, 2016, 11:31:16 PM9/13/16
to material...@googlegroups.com

What’re the design and process requirements? Could you be specific??

 

Thanks.

 

Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 

 


From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Harikrishna Desiti
Sent: Tuesday, September 13, 2016 5:05 AM
To: material...@googlegroups.com
Subject: [MW:25378] Would 317L grade stainless instead against 316L

 

Dear sir / experts, 

                          

We are now at the stage of selection of some analyzers, Would I used 317L grade stainless instead against 316L grade stainless. 

 

 

Thanks & Regards..........?

 

HARIKRUSHNA DESITI

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAhim5%2BKcFPVRDLHkSVj5pg2JNYhpyUp1DYX7h6PV_dvVbc_PQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Harikrishna Desiti

unread,
Sep 14, 2016, 1:42:23 AM9/14/16
to material...@googlegroups.com

Handrail and process GTAW


On 14-Sep-2016 9:01 am, "pgoswami" <pgos...@quickclic.net> wrote:

What’re the design and process requirements? Could you be specific??

 

Thanks.

 

Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Harikrishna Desiti
Sent: Tuesday, September 13, 2016 5:05 AM
To: materials-welding@googlegroups.com
Subject: [MW:25378] Would 317L grade stainless instead against 316L

 

Dear sir / experts, 

                          

We are now at the stage of selection of some analyzers, Would I used 317L grade stainless instead against 316L grade stainless. 

 

 

Thanks & Regards..........?

 

HARIKRUSHNA DESITI

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAGx14oqpUXdMvX7tzuaKp0oBAAAAAA%3D%3D%40quickclic.net.
Reply all
Reply to author
Forward
0 new messages