What is full form of SA in SA516

712 views
Skip to first unread message

Aakash

unread,
Oct 14, 2019, 6:44:23 AM10/14/19
to Materials & Welding
Like Astm it's starts with A.
Please reply ?

Kamal Basha

unread,
Oct 15, 2019, 1:05:58 AM10/15/19
to material...@googlegroups.com
A means ferrous, iam correct friends

On Mon, 14 Oct 2019, 1:44 p.m. Aakash, <haren...@gmail.com> wrote:
Like Astm it's starts with A.
Please reply ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be20054f-c854-4ba7-8a79-1174c5cee752%40googlegroups.com.

SARAVANAN KRISHNAN

unread,
Oct 15, 2019, 6:49:05 AM10/15/19
to material...@googlegroups.com
Hi Akash.

ASTM-tested material will come A 516 grade 60 like this.After that ASME adopted that material will come SA 516 gr 60.

On Mon, Oct 14, 2019 at 1:44 PM Aakash <haren...@gmail.com> wrote:
Like Astm it's starts with A.
Please reply ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be20054f-c854-4ba7-8a79-1174c5cee752%40googlegroups.com.


--
K. SARAVANAN. BE, ME (WELDING TECHNOLOGY)
     WELDING ENGINEER,
     BLACKCAT ENGINEERING  WLL,
     DOHA ,QATAR.
     MOBILE: +974-77466433. INDIA- +91 8939999299.

Mohamed Elsahhar

unread,
Oct 15, 2019, 6:49:05 AM10/15/19
to material...@googlegroups.com
Hi Guys, 

SA516 means the material specification A516 (ASTM A516) Is listed under ASME code section II, for that put S before A516 to specify the material listed under ASME to become SA516. and can check the material specification from ASME II sec A

Best Regards,
M. Elsahhar
Sr. QA/QC Engineer 

Ramesh

unread,
Oct 15, 2019, 6:49:08 AM10/15/19
to material...@googlegroups.com

"A" is an ASTM designation for materials indicating that the iron content is 50% or more (ferrous material). If the iron content is less than 50%, the next abundant element would determine the alloy type (and the specification generally would start with the letter B).

If an ASTM material specification has been adopted by ASME, an "S" is added to the designation.

The SA (SA-516) means it is a ferrous material specification from ASTM, that has been adopted for Code use by ASME. 

source : AWS.org


Dont look for exact expansion for S & A, like S means Steel and  A means Authority. 

Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



Ashok Rai

unread,
Oct 16, 2019, 11:28:13 PM10/16/19
to material...@googlegroups.com
Dear All,

Adding to Rameshkannan Devaraj's explanation, please note:

‘SA’ is a prefix of the ASME specification, whereas ‘A’ is prefix from ASTM. 
The ASME SA516 is a part of the ASME Boiler and Pressure Vessel Code (BPVC),
 a standard which governs the use of carbon steel in weldable industrial boilers and pressure vessels. 
Material specifications for SA materials can be found In Section II Part A.  
Further, for the non-ferrous material the prefix ‘SB’ is used which can be found in Section II Part B.  
Hope this clarifies  your query.  
Thanks & regards
Ashok Rai