Hi all 

  We have a pqr qualified without backing and back weld, we have prepared a WPS without back weld, can I use the single WPS for joints with back weld 

Kamal Basha

unread,
May 19, 2019, 5:09:00 AM5/19/19
to material...@googlegroups.com
Joints is non essential variable. So can go with back weld..  if iam wrong please let me know.

On Sun, 19 May 2019, 11:04 a.m. Raju Kandula, <rgka...@gmail.com> wrote:
Hi all 

  We have a pqr qualified without backing and back weld, we have prepared a WPS without back weld, can I use the single WPS for joints with back weld 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALwNT%2B_AoaeESuhU3J3O%3DVJS%3DK5X_t268_TsLOoKS4dRFusqxA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

MAGHROUD Moussa

unread,
May 21, 2019, 5:34:12 AM5/21/19
to material...@googlegroups.com
Yes. 



Envoyé depuis mon smartphone Samsung Galaxy.