WPS reference on PQR-

95 views
Skip to first unread message

Kannayeram Gnanapandithan

unread,
Mar 13, 2017, 11:40:20 PM3/13/17
to materials-welding
ASME SECTION IX,
QW-200.1
                   The WPS shall  reference the supporting Procedure Qualification Record
QW-200.2
                 The completed PQR shall document all Essential and whenrequired supplementary essential variables

     Nowhere it is mentioned that PQR shall reference the WPS
But some client?Auditors insists to mention the WPS no on PQR,  Why, when Code does not address it??
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

Raghuram Bathula

unread,
Mar 13, 2017, 11:48:37 PM3/13/17
to Materials-Welding
preliminary welding procedures are written for providing specific information to all during qualification. It is not necessary to indicate the pWPS/WPS numbers on the PQR. 
we can write 'n' number of WPS's supporting one PQR. do we write all of these WPS numbers on PQR?
refer interpretation # IX-10-22

-

Perumal Govindan

unread,
Mar 14, 2017, 12:05:29 AM3/14/17
to material...@googlegroups.com

Dear Sir,

I believe if the PQR was conducted followed by a Client approved pWPS, the WPS number might be indicated.

Regards
P Govindan

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNUAgjWQa0WVPPoxPZ1%2BDg94yEdEOd%2BfJWsCtgNW2%2BVzA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Kannayeram Gnanapandithan

unread,
Mar 14, 2017, 12:50:04 AM3/14/17
to materials-welding
There is no Preliminary WPS addressed in Code?

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Mar 14, 2017 at 9:17 AM, Raghuram Bathula <raghura...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (raghura...@gmail.com) Add cleanup rule | More info

preliminary welding procedures are written for providing specific information to all during qualification. It is not necessary to indicate the pWPS/WPS numbers on the PQR. 
we can write 'n' number of WPS's supporting one PQR. do we write all of these WPS numbers on PQR?
refer interpretation # IX-10-22

On 14 March 2017 at 07:36, Kannayeram Gnanapandithan <kgpan...@gmail.com> wrote:

-

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Vishal Sharma

unread,
Mar 14, 2017, 6:37:06 AM3/14/17
to material...@googlegroups.com
Please check code suggested format. Following good engineering practice pWPS/WPS number to be written. As client insists, you have to follow instruction of client.

Br,
Vishal Sharma

Kannayeram Gnanapandithan

unread,
Mar 14, 2017, 7:45:55 AM3/14/17
to materials-welding
Not necessary. We are authorised to qualify PQR/WPS as per code requirement. Go with Raghuram. Format is only suggested and not necessary to follow, but we can make ours in which all essential, non essential, if required supplementary essential variable are to be addressed. 

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Mar 14, 2017 at 2:31 PM, Vishal Sharma <vishalsharm...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (vishalsharma.sharma225@gmail.com) Add cleanup rule | More info

Please check code suggested format. Following good engineering practice pWPS/WPS number to be written. As client insists, you have to follow instruction of client.

Br,
Vishal Sharma
On Tue, Mar 14, 2017 at 8:19 AM, Kannayeram Gnanapandithan <kgpan...@gmail.com> wrote:

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
BPVC-IX-Interp_Stnd-62_2012.pdf
Reply all
Reply to author
Forward
0 new messages